Home - Knowledge - Details

What Is the Application of Cored Wire in Casting Steelmaking?

What a Cored Wire Is

A cored wire is a continuous steel tube filled with a powdered or granular additive. The sheath is a low-carbon steel strip formed into a tube and closed by seam overlap or lock, and the core carries the active material: calcium silicon, pure calcium, ferro-calcium, aluminium, ferrotitanium, carbon, sulphur or a rare-earth blend. Diameters typically run from about 9 mm to 16 mm, with sheath thickness in the 0.3 mm to 0.5 mm range, and the fill ratio is quoted as grams of core material per metre of wire. The wire is fed into a ladle of liquid steel at a controlled speed by a wire feeder, so the addition is made below the slag layer instead of on top of it.

Inclusion Shape Control in Continuous Casting

The main reason steelmakers use cored wire is inclusion morphology. In aluminium-killed steel the deoxidation product is solid alumina, which stays solid at casting temperature and tends to build up at the tundish nozzle and cause clogging or surface defects. A calcium silicon or calcium wire addition converts solid alumina into liquid calcium aluminate, which stays deformable through the casting and rolling window, reducing nozzle blockage and improving the internal quality of slabs and billets. Clogging, together with the resulting flow pattern in the mould, is one of the direct causes of longitudinal surface cracks and macrosegregation. Because the wire is fed deep into the ladle, the calcium reacts with the inclusions in the steel rather than with the slag, so a given mass of calcium does more useful work.

Alloying Yield and Cost Reduction

Feeding an additive as cored wire rather than as bulk lumps raises recovery and cuts consumption. Reactive elements such as calcium, titanium and rare earths have a strong affinity for oxygen and are partly lost if they are added to the tapping stream or to the slag surface. Enclosing the material inside a steel sheath delays its exposure until it is below the slag-metal interface, so a larger fraction of the addition dissolves in the steel. Steelmakers see this as a lower consumption of the alloying addition, a more predictable final composition, and fewer re-treatments after the heat has been tapped.

Common Wire Types and Process Parameters

Wire type Core material Main purpose
Calcium silicon wire Ca-Si alloy powder Inclusion modification, desulphurisation assistance
Pure calcium wire Metallic calcium Alumina modification in aluminium-killed steel
Aluminium wire Aluminium powder or granules Final deoxidation, aluminium trimming
Carbon wire Graphite or coke powder Carbon correction in low-carbon heats
Ferrotitanium wire Fe-Ti powder Titanium alloying, grain refinement

Selecting and Verifying Cored Wire

Wire selection starts from the treatment objective, the heat size and the ladle geometry. Feed speed and injection depth are then set so that the sheath dissolves in the lower half of the ladle, giving enough residence time for the reaction products to float out before casting begins. Sheath thickness and fill consistency determine whether the wire feeds smoothly or breaks in the feeder. Buyers therefore check fill weight per metre, core chemistry, sheath thickness and moisture, and they expect the wire to be wound on a spool or in a coil that will run without kinks. Powder that has absorbed moisture can cause popping in the ladle, so packaging is normally moisture-barrier lined and the wire is used within a stated shelf life.

Frequently Asked Questions

Q: What is the main application of cored wire in steelmaking?
A: Inclusion shape control. Calcium-bearing wire converts solid alumina inclusions into liquid calcium aluminate, which reduces nozzle clogging and improves cast surface and internal quality.

Q: Why is cored wire used instead of adding the alloy in bulk?
A: Because the sheath takes the additive below the slag layer, recovery of reactive elements such as calcium, titanium and rare earths is higher, so consumption per heat and cost per tonne of steel fall.

Q: Which wire is used for inclusion modification in aluminium-killed steel?
A: Calcium silicon wire is the most common choice, with pure calcium wire used where a lower silicon addition is required in the final chemistry.

Q: How is the feed rate decided?
A: It is set from heat weight, ladle depth, wire diameter and core fill ratio so that the sheath dissolves below the slag layer and the reaction products have time to float before casting.

Q: What is checked on receipt of a cored wire shipment?
A: Fill weight per metre, core chemistry, sheath thickness and condition, moisture level and coil integrity, because these are the parameters that decide whether the wire will feed reliably.

Q: Does cored wire also desulphurise?
A: Calcium-bearing wire does contribute to desulphurisation, but for deep sulphur reduction it is normally used together with a ladle treatment such as a calcium aluminate flux or a vacuum or stirring step.